34CrNiMo6 Steel
Steel name: 34CrNiMo6
Table No.:1731
DIN designation: 34CrNiMo6
Mat.No. (Wr.Nr.) designation: 1.6582
AISI/SAE designation: 4340
EN designation: 34CrNiMo6
UNI designation: 35NiCrMo6
AFNOR designation: 35NCD6
BS designation: 817M40
GOST designation: 38Ch2N2MA
Chemical composition in weight %: 0.30-0.38% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
Steel group: Alloy steels
Applications: No data
Note: Ac1=715 C, Ac3=770 C, Ms=320 C, Mf=100 C.
Reference: Not shown in this demo version.
Heat Treatment
Quenching: 870 C/oil, polymer
Tempering: 600-650 C/air
Table Tempering Temperature - Hardness - Mechanical Properties
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.