16NiCr4 Steel
Steel name: 16NiCr4
Table No.: 1930
DIN designation: 15CrNi6
Mat.No. (Wr.Nr.) designation: 1.5714
AISI/SAE designation: 3215 appr.
EN designation: 16NiCr4
UNI designation: 16NiCr4
AFNOR designation: 16NC4
BS designation: 637M17
GOST designation: 16HGN
Chemical composition in weight %: No data
Steel group: Case hardening steels
Applications: No data
Note: Ac1=735, Ac3=825, Ms (core)=380 C, Ms (carburizing surface)=180 C.
Reference: Not shown in this demo version.
Core hardening: 840-880 C/oil, polymer, salt bath
Carburizing: 870-950 C
Tempering: 150-200 C
Table Tempering Temperature - Hardness - Mechanical Properties
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.