819B Steel
Steel name: 819B
Diagram No.: 1981
DIN designation: 36NiCrMo16
Mat.No. (Wr.Nr.) designation: 1.6773
EN designation: 36NiCrMo16
AFNOR designation: 36NiCrMo16 (former 35NCD16)
Chemical composition in weight %: 0.35% C, 1.70% Cr, 0.30% Mo, 3.80% Ni
Steel group: Plastic mould tool steels
Properties: No data
Applications: Bolsters for drop stamps. Moulds for manufacturing plastic materials.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: Preheat to 650°C, raise to 875°C, air cool or gas pressure quench.
Tempering: See the diagram.
Diagram note: 1 cm thick test piece.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.