54SiCrV6 Steel
Steel name: 54SiCrV6
Diagram No.: 1984
DIN designation: 54SiCrV6
Mat.No. (Wr.Nr.) designation: 1.8152
AISI/SAE designation: ~92V54
Chemical composition in weight %: 0.56% C, 1.45% Si, 0.70% Mn, max. 0.010% P, max. 0.010% S, 0.65% Cr, 0.16% V
Steel group: Alloy steels
Properties: No data
Applications: Si-Cr-V alloyed quenched and tempered steel for production of springs with extraordinary small sag tendency, especially of valve and high-stressed automotive suspension springs, produced by cold and hot forming
Reference: Not shown in this demo version.
Heat Treatment
Hardening: min. 840°C/oil
Tempering: 375-500°C/air
Diagram note: No data
Diagram Tempering Temperature - Mechanical Properties
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.