523C VIP Steel
Steel name: 523C VIP
Diagram No.: 2024
Chemical composition in weight %: 0.27% C, 0.25% Si, 1.50% Mn, 1.40% Cr, 0.55% Mo, 1.10% Ni, +others
Steel group: Plastic mould tool steels
Properties: 523C VIP is finish heat-treated in the delivery condition. Additional Heat-treatment may be necessary for stress relieving after deep milling operation and for volume welding operation.
Applications: Moulds for plastic injection moulding, dies for plastic extrusion, general constructional parts -like machine components requiring improved fatigue strength and reliability.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 840-880 C/oil (down to 150 C).
Tempering: 550 -580 C, cooling down on air to 450°C.
Diagram note: No data
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.