934B VIP Steel
Steel name: 934B VIP
Diagram No.: 2034
Mat.No. (Wr.Nr.) designation: 1.2344
EN designation: X40CrMoV5-1
AISI/SAE designation: H13
Chemical composition in weight %: 0.38% C, 0.80% Si, 0.40% Mn, <0.020% P, <0.003% S, 5.00% Cr, 1.40% Mo, 1.00% V
Steel group: Hot work tool steels
Properties: No data
Applications: For highly stressed hot working tools as extrusion dies, components for die casting moulds, drop forging dies and dies for forging machines, hot shear tools, mandrels and containers for (light) metal extrusion, mouldsfor plastic injection when processing of plastics with higher glass fibrecontent, high polished and extra wear resistentplastic moulds. Generally for plastic molds and tools were high toughness and best surface quality is needed, 934E VIP, is to prefer.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 1010-1030 C/vacuum(down to 150°C).
Tempering: See the diagram. Cool down on air to450°C.
Diagram note: No data
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.