DCF Steel

Steel name: DCF
Diagram No.: 2039
Chemical composition in weight %: 0.40% C, 1.00% Si, 0.60% Mn, 5.25% Cr, 1.50% Mo, 1.00% V
Steel group: Plstic mould tool steels
Properties: Finkl DCF is recommended for plastic injection molding of abrasive materials, e.g. thermoplastic and thermosetting grades, where polishability is not important. DCF is also recommended for mold components that are subjected to elevated temperatures such as hot runner manifolds.
Applications: No data
Reference: Not shown in this demo version.

Heat Treatment
Hardening: No data.
Tempering: See the diagram.
Diagram note: Finkl DCF is supplied in the pre-hardened condition and does not require heat treatment before use. Especially complex molds and dies can be stress relieved at 1000°F for one hour per inch thickness to minimize distortion before final machining.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.