16MnCr5 Steel

Steel name: 16MnCr5
Table No.: 2078
DIN designation: 16MnCr5
Mat. No. designation: 1.7131
Chemical composition in weight %: 0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.035% P, max. 0.035% S, 0.80-1.10% Cr
EN designation: 16MnCr5
AISI/SAE designation: 5115
UNI designation: 16MnCr5
AFNOR designation: 16MC
GOST designation: 16HG
GB designation: 15CrMn
Steel group: Case hardening steels
Properties: No data
Applications: No data
Reference: Not shown in this demo version.

Heat Treatment
Core hardening: 860-900 C/oil, polymer, salt bath.
Carbonitriding: 750-930/gas.
Carburizing: 880-980 C.
Hardening (carburizing surface): 810-840/oil, polymer, salt bath.
Tempering: 150-200 C.

Table Tempering Temperature - Hardness - Mechanical Properties

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.