52SiCrNi5 Steel
Steel name: 52SiCrNi5
Table No.: 2098
DIN designation: 52SiCrNi5
Mat.No. (Wr.Nr.) designation: 1.7117
AISI/SAE designation: No data
EN designation: 52SiCrNi5
UNI designation: 52SiCrNi5
AFNOR designation: 52SiCrNi5
GB designation: ZG50CrMo
GOST designation: 52XHC
Chemical composition in weight %: 0.49-0.56% C, 1.20-1.50% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr, 0.50-0.70% Ni
Steel group: Alloyed steel
Applications: No data
Note: Ac1=760 C, Ac3=810 C, Ms=270 C, Mf=50 C.
Reference: Not shown in this demo version.
Heat Treatment
Quenching: 840-870 C/oil or polymer
Tempering: 400-450 C
Table Tempering Temperature - Hardness - Mechanical Properties
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.