M7 Steel
Steel name: M7
Diagram No.: 2173
Mat.No. (Wr.Nr.) designation: 1.3348
AISI/SAE designation: M7
Chemical composition in weight %: 1.02% C, 0.40% Si, 0.30% Mn, 3.80% Cr, 8.60% Mo, 1.90% V, 1.80% W
Steel group: High speed tool steels
Properties: No data
Applications: Taps, twist drills, reamers, milling tools, broaches, cold extrusion dies.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: Hardening temperature of 2000 to 2210°F (1170 to 1210°C); quench in: oil, salt bath at 930 to 1020°F (500 to 550°C), or vacuum. The upper temperature range should be used for parts of simple geometry, the lower range for more complex tooling. For cold work tooling, lower temperatures are of importance for improved toughness.
Tempering: Slowly and uniformly heat to the appropriate tempering temperature immediately after the hardening operation. Once the temperature of the tool has been equalized, a soaking period of one hour per inch (25 mm) of workpiece thickness is required, but not less than 2 hours. First and second tempers should be used to reach the desired hardness level, and the third selected for additional stress relief at 85 - 120°F (30 to 50°C) below the highest tempering temperature. Intermittent cooling, in air, between tempers is required for a minimum of 1 hour. Obtainable hardness of 64 to 66 HRC.
Diagram note: Hardening temperature: 2175°F (1190°C) Specimen size: square cross section 20 mm.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.