N695 Steel

Steel name: N695
Diagram No.: 2185
DIN designation: X105CrMo17
Mat.No. (Wr.Nr.) designation: ~1.4125
AISI/SAE designation: 440C
UNI designation: X102CrMo17 KU
JIS designation: SUS 440C
AFNOR designation: Z100CD17
Chemical composition in weight %: 1.05% C, 0.40% Si, 0.40% Mn, 17.00% Cr, 0.50% Mo
Steel group: Chromium stainless steels
Properties: No data
Applications: Balls, rollers, needles and rings for corrosion resistant bearings.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1000 to 1050°C /oil
Tempering: 100 to 200°C
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.