Vanadis 10 Steel

Steel name: Vanadis 10
Diagram No.: 2189
Chemical composition in weight %: 2.90% C, 0.50% Si, 0.50% Mn, 8.00% Cr, 1.50% Mo, 9.80% V
Steel group: PM tool steels
Properties: No data
Applications: No data
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1020–1100°C (1870–2010°F)/30 min/air/gas, vacuum, martempering bath or fluidized bed at 200– 350°C (390–660°F) whereby 350°C (660°F) is preferred.
Tempering: Choose the tempering temperature according to the hardness required by reference to the tempering graph. Temper twice with intermediate cooling to room temperature. Lowest tempering temperature 180°C (360°F). Holding time at temperature minimum 2 hours. At a hardening temperature of 1100°C (2010°F) or higher Uddeholm Vanadis 10 SuperClean should be tempered at minimum 525°C (980°F) in order to reduce the amount of retained.
Diagram note: Holding time 30 min. Air-cooling.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.