Chemical composition in weight %: 0.60% C, 0.35% Si, 0.80% Mn, 4.50% Cr, 0.50% Mo, 0.20% V
Steel group: Alloy steels
Properties: No data
Applications: No data
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Pre-heating temperature: 600–700°C (1110– 1290°F). Austenitizing temperature: 950–970°C (1740– 1780°F), normally 960°C (1760°F). Holding time: 30–45 minutes. Quenching media: High speed gas/circulating atmosphere.Salt bath 200–550°C (390–1020°F). Fluidized bed 200–550°C (390–1020°F).
Note 1: Quenching should not be interrupted until the part has cooled down to 25°C (75°F). Otherwise the part may shrink after tempering.
Note 2: Temper immediately after quenching.
Note 3: Quenching in oil is not recommended.
Tempering: The tempering temperature for the required hardness may be determined by means of the tempering graph. Temper twice. Lowest tempering temperature 200°C (390°F). Holding time at temperature minimum 2 hours.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.