HS2-9-1 Steel

Steel name: HS2-9-1
Diagram No.: 220
DIN designation: HS2-9-1
Mat.No. (Wr.Nr.) designation: ~1.3346
AISI/SAE designation: M1
Chemical composition in weight %: 0.84% C, 0.40% Si, 0.30% Mn, 3.80% Cr, 8.50% Mo, 1.20% V, 1.80% W
Steel group: High speed steels
Applications: Taps, twist drills, reamers, milling tools, broaching tools.
Note: Tempering chart: Hardening temperature: 1190°C (2174°F). specimen size: square 20 mm.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1170 to 1210oC/oil, salt bath, vacuum
Tempering: See the diagram

Tempering Diagram


Click the image to enlarge the diagram.

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.