1.2311 Steel

Steel name: 1.2311
Diagram No.: 2204
Mat.No. (Wr.Nr.) designation: 1.2311
DIN designation: 40CrMnMo7
AISI/SAE designation: ~P20
Chemical composition in weight %: 0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.003% S, 2.00% Cr, 0.20% Mo
Steel group: Mould steels
Properties: Quenched and tempered to 280-325 HB = 900-1100 N/mm2, annealed as requested.
Applications: Small and medium-sized injection and compression moulds, mould frames up to 400 mm thickness.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Temperature: 880°C. Duration: 1 min. per 1 mm wall thickness.
Tempering: Temperature: see curve. Duration: 1 h per 25 mm wall thickness. Cooling: air.
Diagram note: Average values for samples dia. 25 x 50 mm long, oil hardened at 880°C. N/mm2 and HB converted from HRC.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.