1.2316 Steel
Steel name: 1.2316
Diagram No.: 2206
Mat.No. (Wr.Nr.) designation: 1.2316
DIN designation: X36CrMo17
Chemical composition in weight %: 0.28% C, 0.30% Si, 0.35% Mn, 0.030% P, 0.003% S, 14.20% Cr, 1.10% Mo, 0.50% Ni
Steel group: Corrosion resistant tool steels
Properties: Modified, corrosion resistant mould steel, suitable for polishing, chatter and machining.
Applications: Injection moulds, mould inserts, wide slot nozzles, profiled dies, extrusion tools, calibration tools, and concentric bolsters for PVC urea resins and additives and blow moulds.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: Temperature: 1030°C Duration: 1 min. per 1 mm wall thickness.
Tempering: Temperature: see curve. Duration: 1 h per 25 mm wall. thickness Cooling: air.
Diagram note: Average values for samples dia. 25 x 50 mm long, oil hardened at 1030°C. N/mm2 and HB converted from HRC.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.