1.2738 HH Steel
Steel name: 1.2738 HH
Diagram No.: 2212
Mat.No. (Wr.Nr.) designation: 1.2738 HH
Chemical composition in weight %: 0.25-0.35% C, 0.30-0.60% Si, 1.40-1.70% Mn, 1.40-1.80% Cr, 0.40-0.60% Mo, 0.20-0.60% Ni
Steel group: Tool steel for plastics
Properties: KeyLos PLUS is a special and innovative pre-hardened alloyed steel, suitable for the manufacture of a large amount of injection moulds. This steel has been designed to enhance in the moulds the following characteristics: high degree of homogeneity of hardness and toughness in the section; good weldability, in case of repair; better machinability, reduction in cutting insert cost, shorter machining time; better surface quality and polishability, due to the high cleanliness and fine microstructure; shorter injection cycle time, due to the high thermal conductivity. KeyLos PLUS is obtained through a special 'super clean' manufacturing process and a special suited heat treatment process.
Applications: Plastic moulding: medium and big sized moulds for the automotive industry; moulds for the food industry; moulds for rubber pressing; pressure moulds (SmC, BmC); bolsters. exTruSion: dies and gauges for pVC extrusion; mechanical parts for extrusion presses.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: Temperature: 900°C. Soaking time: 60 min every 25 mm thickness. Cooling: Polymer or water quench.
Tempering: Temperature: See the graph. Soaking time: 60 min every 25 mm thickness. Cooling: Room temperature.
Diagram note: Tempering curve of a sample which has been austenitised at 900 C.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.