1.2343/1.2343 ESR Steel

Steel name: 1.2343/1.2343 ESR
Diagram No.: 2222
Mat.No. (Wr.Nr.) designation: 1.2343/1.2343 ESR
DIN designation: X38CrMoV5-1
AISI/SAE designation: H11/H11 ESR
Chemical composition in weight %: 0.38% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.20% Mo, 0.40% V
Steel group: Hot work tool steels
Properties: High-alloy hot-work steel with high toughness and heat resistance, hot cracks resistance and good thermal conductivity; for very high requirements available in grade *ESR (Electro-Slag Remelted).
Applications: Moulding plates and inserts for plastic injection mould tools; ESR for die casting applications (Al, Mg, Zn).
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1000 to 1040 °C keep curing temperature for 15 to 30 minutes quenching in water/oil/air, obtainable hardness: 50-56 HRC.
Tempering: Slow heating to tempering temperature immediately after hardening; minimum time in furnace: 1 hour per 20 mm part thickness; repeated tempering is recommended.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.