1.2714 HH Steel
Steel name: 1.2714 HH
Diagram No.: 2227
Mat.No. (Wr.Nr.) designation: 1.2714 HH
DIN designation: 56NiCrMoV7
AISI/SAE designation: L6
Chemical composition in weight %: 0.56% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
Steel group: Tool steels
Properties: Steel for through hardening with good heat resistance, high temperature resistance, through hardenability and toughness.
Applications: Large mould tools with high loads at core, moulds for bumpers, dashboards, moulding frames.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 840 to 870°C, 15 to 30 minutes keeping curing temperature quenching in oil/heat bath /air 180 to 220°C, obtainable hardness: 53 HRC.
Tempering: Slow heating to tempering temperature immediately after hardening; minimum time in furnace: 1 hour per 20 mm part thickness.
Diagram note: No data
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.