1.3344 PM (PM23) Steel

Steel name: 1.3344 PM (PM23)
Diagram No.: 2232
Mat.No. (Wr.Nr.) designation: 1.3344 PM (PM23)
DIN designation: PM6-5-3
AISI/SAE designation: M 3-2 (PM)
Chemical composition in weight %: 1.25% C, 0.30% Si, 0.30% Mn, 4.00% Cr, 5.00% Mo, 3.00% V, 6.20% W
Steel group: PM steels
Properties: Powder metallurgy high-speed steel with good machinability, high resistance to adhesive and abrasive wear, with optimal toughness due to the uniform and fine carbide structure, very good through hardenability and high dimensional stability.
Applications: Blocks for eroding, cutting punches and dies with particularly durable edges, inserts with excellent wear resistance.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Curing temperature: see tempering chart quenching in oil/compressed gas/air/hot bath, obtainable hardness: 64-66 HRC.
Tempering: Slow heating to tempering temperature (in order to avoid formation of cracks) immediately after hardening; tempering three times is recommended.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.