M V10 PM Steel

Steel name: M V10 PM
Diagram No.: 2234
AISI/SAE designation: A11 (PM)
Chemical composition in weight %: 2.45% C, 0.90% Si, 0.50% Mn, 5.20% Cr, 1.30% Mo, 0.75% V
Steel group: PM steels
Properties: Powder metallurgical high-speed steel with optimal dimensional accuracy after the heat treatment. Highest abrasive wear resistance and excellent toughness. Good machinability through a homogeneous microstructure.
Applications: Blocks for eroding, dies and cutting punches with extreme requirements, fine blanking punches, pressing punches for sinter press tools.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Curing temperature: see tempering chart quenching in oil/compressed gas/air/hot bath, obtainable hardness: 60-63 HRC.
Tempering: Slow heating to tempering temperature (to avoid forming of cracks) immediately after hardening; triple tempering is recommended.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.