MLX 19 Steel

Steel name: MLX 19
Diagram No.: 2236
AMS designation: 5955 (bar and forging)
DIN designation: X1NiCrMoAlTi12-10-2
UNS designation: S11902
Chemical composition in weight %: max. 0.02% C, max. 0.25% Si, max. 0.25% Mn, max. 0.015% P, max. 0.010% S, 9.50-10.50% Cr, 1.75-2.25% Mo, 11.50-13.00% Ni, 0.95-1.50% Ti, 1.30-1.70% Al, max. 0.01% N
Steel group: Ultra high strength stainless steels
Properties: The use of Precipitation Hardening Stainless Steels for structural parts in industrial components has been in place for a while considering their superior environmental robustness.
Applications: Aerospace parts, motorsport, defense - missiles, fastening systems.
Reference: Not shown in this demo version.

Heat Treatment
Solution heat treatment: 850°C ± 14°C (1560 °F ± 25°F). Quenching in water. Cooling to -73 °C (-100 °F) for 8 hours.
Diagram note: No data

Properties depending on ageing time and temperature - UTS

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.