X15TN Steel

Steel name: X15TN
Diagram No.: 2243
Mat.No. (Wr.Nr.) designation: 1.4123
DIN designation: X40CrMoVN16-2
UNS designation: S42025
Chemical composition in weight %: 0.37-0.45% Mn, max. 0.60% Si, max. 0.60% Mn, 15.00-16.50% Cr, 1.50-1.90% Mo, max. 0.30% Ni, 0.20-0.40% V, 0.16-0.26% N
Steel group: Martensitic steels
Properties: Partial substitution of carbon with nitrogen. For steels containing 13-17 % of Cr, the addition of nitrogen through a conventional melting method allows a saturation content of ca 0.20 %. In combination with 0.4% to 0.5% carbon.
Applications: Fuel injection, pollution control systems in abrasive / corrosive environments (biofuels, combustion gases), cutting blades with high requirements on corrosion resistance, surgical instruments, mold components for synthetic material processing, glassware molds.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 980 °C and 1080 °C, gas or oil cooling.
Tempering: 180 C, 525 C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.