ASSAB 705 Steel

Steel name: ASSAB 705
Diagram No.: 2246
Mat.No. (Wr.Nr.) designation: 1.6582
DIN designation: 34CrNiMo6
AISI/SAE designation: 4340
Chemical composition in weight %: 0.40% C, 0.70% Mn, 0.80% Cr, 0.25% Mo, 1.80% Ni
Steel group: Alloyed steels
Properties: ASSAB 705 is machinery steel with unique machinability. ASSAB 705 is supplied as quenched and tempered that enhances hardness and toughness distribution.
Applications: ASSAB 705 is an alloyed machinery steel with good hardenability also in large cross sections. It combines high strength with best toughness.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 880-935 C, quench media 100% water.
Tempering: 600-670 C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.