HS6-5-2 Steel
Steel name: HS6-5-2
Diagram No.: 225
DIN designation: HS6-5-2
Mat.No. (Wr.Nr.) designation: ~1.3339
AISI/SAE designation: M2 reg. C
Chemical composition in weight %: 0.85% C, 0.35% Si, 0.25% Mn, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W
Steel group: High speed steels
Applications: Taps, twist drills, reamers, broaching tools, metal saws, milling tools of all types, wood working tools, cold work tools.
Tempering chart: Hardening temparature: 1220°C (2228°F). specimen size: square 20 mm.
Reference: Website Bohler Edelstahl, Austria, 2008.
Heat Treatment
Hardening: 1190 to 1230oC/oil, salt bath, vacuum
Tempering: See the diagram
Tempering Diagram
Click the image to enlarge the diagram.
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.