K455 Steel
Steel name: K455
Diagram No.: 2252
Mat.No. (Wr.Nr.) designation: ~1.2550
DIN designation: ~60WCrV7
AISI/SAE designation: ~S1
Chemical composition in weight %: 0.63% C, 0.605 Si, 0.30% Mn, 1.10% Cr, 0.18% V, 2.00% W
Steel group: Cold work tool steels
Properties: No data
Applications: Cutting tools (dies and punches) for the processing of plate; cold punches and shear blades; woodworking, coining and pneumatic tools. Hot work tools for use at moderate heat.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 870 to 900 °C. Oil, Holding time after temperature equalization: 15 to 30 minutes.
Tempering: After hardening, tempering to the desired working hardness, see tempering chart.
Diagram note: Hardening temperature: 890C/1634F. Specimen size: square 20 mm.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.