K605 Steel

Steel name: K605
Diagram No.: 2255
Mat.No. (Wr.Nr.) designation: ~1.2721
DIN designation: ~50NiCr13
SIS designation: ~2550
Chemical composition in weight %: 0.55% C, 0.30% Si, 0.40% Mn, 1.00% Cr, 0.25% Mo, 3.00% Ni
Steel group: Cold work tool steels
Properties: Cold work tool steel with high thoughness and full hardenability, for air hardening.
Applications: Highly stres sed coi ning tools, cut lery dies, hobbing tools, cold she ar bla des for heavy-gauge ma terial, plas tic moulds.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 840 to 870°C / Air, oil. Holding time after temperature equalization: 15 to 30 minutes. Obtainable hardness: 54 - 58 HRC in air, 55 - 59 HRC in oil.
Tempering: Slow heating to tempering temperature immediately after hardening/time in furnace 1 hour for each 20 mm of workpiece thickness but at least 2 hours/cool ing in air. For average hardness figures to beobtained please refer to the tempering chart. For certain cases we recommend to reduce tempering temperature and in crease holding time.
Diagram note: Tempering chart: Hardening tem perature: 850°C. Specimen size: square 20 mm.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.