M100 Steel

Steel name: M100
Diagram No.: 2258
Mat.No. (Wr.Nr.) designation: 1.2162
DIN designation: 21MnCr5
AISI/SAE designation: ~5120, ~5120H
JIS designation: ~SCR420H
Chemical composition in weight %: 0.20% C, 0.30% Si, 1.20% Mn, 1.10% Cr
Steel group: Plastic mould steels
Properties: Mn-Cr-case hardening steel for plastic moulds. Good machinability and polishability, hobbing is possible.
Applications: For moulds of all sizes.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Carburizing temperature or 810 to 840°C (in order tominimize distortion). Cooling from carburizing, and after reheating hardening from core hardening tem perature 810 to 840°C. Quenchant: Oil, salt bath (160 to 250°C).
Tempering: 170 to 210°C / air cooling.
Diagram note: Tempering chart: Hardness values of the case-hardened layer. Hardening temperature: 820°C. Quenchant: Oil.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.