M4 Steel
Steel name: M4
Diagram No.: 226
UNS designation: ~T11304
JIS designation: ~SKH54
AISI/SAE designation: M4
Chemical composition in weight %: 1.33% C, 0.35% Si, 0.30% Mn, 4.30% Cr, 4.00% Mo, 4.10% V, 5.90% W
Steel group: High speed PM steel
Applications: Shaper cutters, hobs, milling cutters, broaching tools of all types, etc.
Tempering chart: specimen size: square 20 mm.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 1150 to 1200oC/oil, salt bath, vacuum
Tempering: See the diagram
Diagram note: Holding time 2 x 2h, specimen size 25 x 20 x 15 mm, austenitizing in salt bath.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.