M314 Extra Steel
Steel name: M314 Extra
Diagram No.: 2264
Chemical composition in weight %: 0.34% C, 0.35% Si, 1.40% Mn, 0.12% S, 16.00% Cr, 0.15% Mo, plus others
Steel group: Mould holder steels
Properties: BÖHLER M314 EXTRA, the corrosion resistant mould frame steel is used for the processing of aggressive plastics, in humid climatic conditions, for applications involving the formation of condensation water, etc.
Applications: Mould holders for the plastics processing and die casting industries as well as ancillary plastics processing tools.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: Holding time 30 minutes / oil.
Tempering: Operating temperatures above 500°C (using the highest tempering temparature) are possible without the risk of any major decrease in hardness. Tempering: 2 x 2 hours. Specimen size: square 20 x 20 mm.
Diagram note: Specimen size: square 20 x 20 mm.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.