W320 ISODISC Steel

Steel name: W320 ISODISC
Diagram No.: 2276
Mat.No. (Wr.Nr.) designation: ~1.2365
DIN designation: 32CrMoV12-28
AISI/SAE designation: ~H10
JIS designation: SKD7
Chemical composition in weight %: 0.31% C, 0.30% Si, 0.35% Mn, 2.90% Cr, 2.70% Mo, 0.50% V
Steel group: Hot work tool steels
Properties: Hot work tool steel fea turing a fine combnation of heat checking resistance, hot strength and im pact strength; ad mits water cooling.
Applications: Highly stressed hot work tools, mainly for the processing of heavy alloys, such as mandrels, dies and containers for metal tube and rod extrusion; hot extrusion tools; tools for the manufacture of hollows, screws, rivets, nuts and bolts. Die casting tools, forming dies, die inserts, hot shear blades.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1010 to 1050°C (1850 to 1922°F) Oil, salt bath (500-550°C / 932-1022°F), Holding time after temperature equalization: 15 to 30 minutes. Obtainable hardness: 52 - 56 HRC
Tempering: Slowheating to tempering temperature immediately after hardening / time in furnace 1 hour for each 20 mm of work piece thickness but at least 2 hours / cooling in air. It is recommended to temper at least twice. A third tempering cycle for the purpose of stress relieving may be advantageous 1st tem pering ap prox. 30°C (86°F) above maximum secondary hardness. 2nd tempering to desired working hardness. The tempering chart shows average tempered hardness values. 3rd for stress relieving at a temperature 30 - 50°C (86 to 122°F) below highest tempering temperature.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.