W360 ISOBLOC Steel

Steel name: W360 ISOBLOC
Diagram No.: 2279
Chemical composition in weight %: 0.50% C, 0.20% Si, 0.25% Mn, 4.50% Cr, 3.00% Mo, 0.55% V
Steel group: Hot work tool steels
Properties: BÖHLER W360 ISOBLOC was developed as a tool steel for dies and punches in warm and hot forging. The steel can be used for a variety of applications where hardness and toughness are required.
Applications: Dies and punches in warm and hot forging. Tooling for high speed presses. Toughness-critical cold work applications. Extrusion tooling, e.g. dies. Core pins and inserts in die-casting dies. Specific applications in the plastic processing sector.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1050 °C (1920 °F)/oil, salt bath 500 bis 550 °C (930 to 1020 °F), air, vacuum furnace with gas quenching. Holding time after through-heating: 15 to 30 minutes.
Tempering: Slowly heat to tempering temperature immediately after hardening. Time in furnace: 1 hour for every 20 mm of workpiece thickness but at least 2 hours. Cool in air. We recommend that the steel be tempered at least 3 times.
Diagram note: Hardening temperature 1050 °C [1920 °F] (Vacuum).

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.