W400 VMR Steel

Steel name: W400 VMR
Diagram No.: 2280
Mat.No. (Wr.Nr.) designation: ~1.2343
DIN designation: ~X37CrMoV5-1
AISI/SAE designation: ~H11
JIS designation: ~SKD6
Chemical composition in weight %: 0.38% C, 0.20% Si, 0.30% Mn, 5.00% Cr, 1.30% Mo, 0.50% V
Steel group: Hot work tool steels
Properties: Good macro- and microstructure with lowest levels of segregation. Lowest gas contents. Lowest levels of unwanted trace elements. Excellent homogeneity and isotropy. Highest degree of cleanliness. Highest toughness. Best polishability. Best thermal conductivity. Highest dimensional stability during heat treatment. Good machinability. Higher working hardness for increased service life (less hot wear, higher hot strength).
Applications: Heavy duty hot work tools and dies, mainly for light alloy processing: mandrels, dies, and containers for metal tube and rod extrusion; hot extrusion equipment; tools and dies for the manufacture of hollow bodies, screws, rivets, nuts and bolts. Die casting equipment, forming dies, die inserts, hot shear blades, and plastic moulding dies.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 980 to 990 °C (1795 to 1815 °F) Oil, salt bath (500 – 550 °C [930 – 1020 °F]), air or vacuum with gas quenching. Holding time after temperature equalization: 15 to 30 minutes. Obtainable hardness: 52 – 54 HRc in oil or salt bath hardening, 50 – 53 HRc in air or vacuum hardening.
Tempering: Slow heating to tempering temperature immediately after hardening/time in furnace 1 hour for each 20 mm (0.79 inch) of workpiece thickness but at least 2 hours/cooling in air. It is recommended to temper at least twice. A third tempering cycle for the purpose of stress relieving may be advantageous. 1st tempering approx. 30 °C (85 °F) above maximum secondary hardness. 2nd tempering to desired working hardness. The tempering chart shows average tempered hardness values. 3rd for stress relieving at a temperature 30 to 50 °C (85 – 120 °F) below highest tempering temperature.
Diagram note: Hardening temperature: 990 °C (1815 °F). Specimen size: square 20 mm (0.79 inch).

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.