Thruhard Diamond-HHH Steel
Steel name: Thruhard Diamond-HHH
Diagram No.: 2292
Chemical composition in weight %: 0.28% C, 0.10% Si, 1.45% Mn, 0.015% P, 0.002% S, 1.25% Cr, 0.70% Mo, 1.05% Ni, 0.15% V
Steel group: Plastic mould steels
Properties: Remelted hardened and tempered plastic mould steel for the most demanding surface fi nish requirements. Thruhard Diamond is based on the successful development of the patented Thruhard Supreme.
Applications: Injection moulding and compression dies with the most demanding surface finish requirements for producing items such as transparent headlight components, automotive trim and radiator grille panels. Ideally suited for interior use both for polished surfaces and for extra fine-grained surfaces.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: Temperature: 880 °C. Duration: 1 minute per mm wall thickness.
Tempering: Temperature: See tempering curve Duration: 1 hour per 25 mm wall thickness. Cooling: Air.
Diagram note: Average values on samples dia. 25 x 50 mm long hardened at 880 ºC in oil. HB converted from HRC.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.