Thruhard Efficient Steel

Steel name: Thruhard Efficient
Diagram No.: 2293
Chemical composition in weight %: 0.30% C, 0.10% Si, 1.45% Mn, 0.20% P, 0.003% S, 1.35% Cr, 0.50% Mo, 0.65% Ni
Steel group: Plastic mould steels
Properties: Mould steel with hardness 280–325 HB or 310-355 HB. Hard chrome plateable, flame and laser hardenable, etch-grainable, nitridable (max. 500 °C). Where there is a requirement for polishability > 320 grit and/or sensitive etch-graining designs (e.g. HNO3, fine or textile graining) we recommend 2738mod.TS(HH). For applications that require a combination of high strength and toughness we recommend grade 2711 ISO-B.
Applications: Compression and injection moulds where higher hardness is needed. Thickness max. 600 mm (width on request).
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Temperature: 880 °C. Duration: 1 minute per mm wall thickness.
Tempering: Temperature: See tempering curve. Duration: 1 hour per 25 mm wall thickness. Cooling: Air.
Diagram note: Average values on samples dia. 25 x 50 mm long hardened at 880 °C in oil. HB converted from HRC.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.