CarTech O1 Steel

Steel name: CarTech O1
Diagram No.: 2299
UNS designation: T31501
AISI/SAE designation: O1
Chemical composition in weight %: 0.90% C, 1.20% Mn, 0.50% Cr, 8.00% Mo, 0.20% V, 0.50% W
Steel group: Tool steels
Properties: CarTech 01 is a manganese-chromium-tungsten, nondeforming, oil hardening general purpose tool and die steel which is safe to harden, even in intricate sections.
Applications: Blanking dies, forming dies, lamination dies, molding dies, trimming dies, broaches, collets, stamps, master tools, spindles, master taps, thread gauges.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 01 may be hardened from temperatures between 1450/1500°F (788/816°C). Endothermic atmospheres should be held to dew point limits between 45/55°F (7/18°C). This wide hardening range makes it possible to fit into many heat treating schedules during the average day. This broad a hardening range supersedes all other references to 01 hardening temperatures previously published.
Tempering: Temper 01 immediately to the desired hardness level. The minimum tempering time is 1 hour at temperature. Be sure to allow sufficient time to allow the material to reach the proper temperature. Sections over 2 inches thick should be tempered one hour per inch.
Diagram note: No data

Effect Tempering Temperature on Hardness

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.