CarTech Micro-Melt A11 Steel

Steel name: CarTech Micro-Melt A11
Diagram No.: 2308
UNS designation: T30311
AISI/SAE designation: A11
Chemical composition in weight %: 2.45% C, 0.90% Si, 0.50% Mn, 0.080% S, 5.30% Cr, 1.30% Mo, 9.50% V
Steel group: PM tool steels
Properties: CarTech Micro-Melt A11 tool steel is a high vanadium tool steel produced using the Carpenter CarTech Micro-Melt powder metal process. This grade possesses wear resistance superior to most other tool steels, including the high speed steels, along with good strength and toughness characteristics.
Applications: Punches, dies for blanking, piercing dies, forming rolls and dies, cold heading, woodworking tools, cold extrusion, slitter knives, shears, pellitizer blades, nozzles, cold extrusion barrels, cold extrusion liners, plastic injection molds, compacting tools, steel mill rolls.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: Micro-Melt A11 tool steel should be heat treated using proper precautions to prevent decarburization. First, preheat to 1500/1550°F (816/843°C), equalize, and transfer to a furnace maintained at the desired hardening temperature. Alternatively, the tool may be preheated in the vacuum furnace that will be used for the austenitizing cycle. Austenitize at 1850/2150°F (1010/1177°C) for 5 - 60 minutes, depending on the austenitizing temperature used. General suggestions for the austenitizing time to be used depending upon the austenitizing temperature chosen are given in the heat treatment table found at the end of this section. For best toughness combined with good wear resistance, austenitize at 1950°F (1066°C) for 30-60 minutes, then air cool to room temperature. Temper immediately to HRC 58/61. For balanced toughness and wear resistance, austenitize at 2050°F (1121°C) for 20 to 40 minutes, fan air cool, oil quench, or salt quench to 1000°F (538°C) followed by an air cool to room temperature. Alternatively, a vacuum furnace with a 4 bar minimum quench capability may be used. Temper immediately to HRC 60/62. For the maximum wear resistance at some sacrifice in toughness, austenitize at 2150°F (1177°C) for 5 to 10 minutes, oil quench. If a vacuum furnace is used, it should have a 4 bar minimum quench capability. Temper immediately to HRC 63/65.
Tempering: Tools should be tempered immediately after completion of the quench, when they have reached room temperature. The tempering temperature may be adjusted according to the hardness desired. Tempering is usually performed in the temperature range of 1000/1100°F (538/593°C). Triple tempering and/or refrigeration at -100°F (-73°C) is suggested when hardening is performed above 2100°F (1149°C). If refrigeration is used, tools should be refrigerated immediately after the first temper.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.