DHA-HS1 Steel
Steel name: DHA-HS1
Diagram No.: 2321
Chemical composition in weight %: 0.37% C, 1.00% Si, 0.35% Mn, 5.00% Cr, 1.25% Mo, 1.00% V
Steel group: Hot work tool steels
Properties: DHA-HS1 is die steel suitable for hot stamping, in which steel sheets heated to high temperatures are press-formed. Due to its high thermal conductivity, the cooling time of products is reduced, and thus the productivity is increased. Moreover, its high softening resistance extends die life.Therefore, DHA-HS1 helps cut costs of hot-stamped products.
Applications: Hot stamping tools.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 1030 C, Gas cooling (6 bar).
Tempering: See the diagram.
Diagram note: Dimensions:10×15×20 mm. Quenching: 1030 C, Gas cooling (6 bar).
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.