DIMO 30M Steel
Steel name: DIMO 30M
Diagram No.: 2324
AISI/SAE designation: ~4130
Chemical composition in weight %: 0.28-0.35% C, 0.15-0.40% Si, 0.75-1.00% Mn, <0.025% P, <0.02% S, 0.60-1.20% Cr, 0.45-0.65% Mo, >0.04% V
Steel group: Plastic mould steels
Properties: DIMO 30H (Holderblock) is a prehardened CrMnMo S-alloyed tool steel.
Applications: DIMO 30H (Holderblock) is a prehardened CrMnMo S-alloyed tool steel for the construction of plastic molds. DIMO 30H is applied by the customers for accessories with such holderblock requirements as ejector plates, supports, clamping plates and housings for diecasting dies.It is characterized by excellent dimensional stability as well as good machinability. It is also suitable for molds with low surface requirements referring to polishability.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 840 - 860 °C (1540 - 1580 °F)/oil; for low wall thicknesses warm bath hardening at 200 - 230 °C (390 - 450 °F) is possible.
Tempering: According to required hardness (min. 1 h/25 mm (1 in) wall thickness).
Diagram note: The values in the diagram are mean values on samples, diameter 20 mm (¾ in), hardened at 850 °C (1560 °F) in oil.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.