DIMO 2738 Steel
Steel name: DIMO 2738
Diagram No.: 2325
Mat.No. (Wr.Nr.) designation: ~1.2738
DIN designation: 40CrMnNiMo8-6-4
Chemical composition in weight %: 0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, <0.025% P, <0.002% S, 1.80-2.10% Cr, 0.15-0.25% Mo, 0.90-1.10% Ni
Steel group: Plastic mould steels
Properties: No data
Applications: DIMO 2738 is a prehardened CrMnNiMo-alloyed tool steel for the construction of plastic molds with superior surface requirements on molds. It is characterized by excellent polishability, photoetchability, spark erosion behaviour and dimensional stability as well as good machinability. DIMO 2738 shows a better through-hardening compared to DIMO 2311.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 840 - 860 °C (1540 - 1580 °F); air cooling or warm bath hardening at 200 - 230 °C (390 - 450 °F).
Tempering: In accordance with tempering diagram to required hardness (min. 1 h/25 mm (1 in) wall thickness).
Diagram note: The values in the diagram are mean values on samples, diameter 25 mm (1 in), length 50 mm (2 in), hardened at 840 °C (1540 °F) on air.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.