DIMO C45 Steel

Steel name: DIMO C45
Diagram No.: 2327
Mat.No. (Wr.Nr.) designation: ~1.1730
DIN designation: C45
Chemical composition in weight %: 0.42-0.50% C, <0.40% Si, 0.50-0.80% Mn, <0.025% P, <0.010% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni <= 0.63
Steel group: Unalloyed carbon tool steels
Properties: DIMO C45 is an unalloyed carbon tool steel for the construction of plastic mold assemblies. DIMO C45 is designed for holderblock applications requiring extensive machining and high dimensional stability as mold assemblies, ejector plates, supports, clamping plates and housings for diecasting dies.
Applications: Unalloyed carbon tool steel for high quality holderblock applications.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 820 - 860 °C (1508 - 1580 °F) / min. 30 min., water.
Tempering: In accordance with tempering diagram to required hardness.
Diagram note: The values in the diagram are mean values on samples, diameter 25 mm (1 in), length 50 mm (2 in), hardened at 800 °C (1470 °F) in water.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.