DIMO 2312 Steel

Steel name: DIMO 2312
Diagram No.: 2331
Mat.No. (Wr.Nr.) designation: 1.2312
DIN designation: 40CMD8+S
AISI/SAE designation: ~P20
Chemical composition in weight %: 0.35-0.45% C, 0.30-0.50% Si, 1.40-1.60% Mn, <0.030% P, 0.050-0.10% S, 1.80-2.00% Cr, 0.15-0.25% Mo
Steel group: Plastic mould steels
Properties: No data
Applications: DIMO 2312 is a hardened CrMnMoS-alloyed tool steel for the construction of plastic molds with lower surface requirements referring to e.g. polishability and photoetchability. DIMO 2312 is characterized by excellent machinability and high dimensional stability. Moreover, it is used by the customers for accessories with holderblock requirements as e.g. ejector plates, supports, clamping plates and housings for diecasting dies.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 840 - 860 °C (1540 - 1580 °F)/oil; for low wall thicknesses air cooling or warm bath hardening at 200 - 230 °C (390 - 450 °F) are possible.
Tempering: In accordance with tempering diagram to required hardness.
Diagram note: The values in the diagram are mean values on samples, diameter 25 mm (1 in), length 50 mm (2 in), hardened at 850 °C (1560 °F) in oil.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.