DILLIDUR 450 Steel

Steel name: DILLIDUR 450
Diagram No.: 2333
Chemical composition in weight %: <0.25% C, <0.70% Si, <1.60% Mn, <0.025% P, <0.010% S, <1.50% Cr, <0.50% Mo, <0.80% Ni, <0.08% V, <0.30% Cu, <0.05% Nb, <0.005% B
Steel group: Wear resistant steels
Properties: DILLIDUR 450 is a wear resistant steel with a nominal hardness of 450 HBW in delivery condition ex works. DILLIDUR 450 is preferentially used by the customers where elevated resistance to wear is required together with good workability and especially good weldability.
Applications: Examples of application: earth moving and loading machines, dredgers, skip cars, conveying plants, trucks, cutting edges, knives and breakers, waste elimination and recycling plants.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: No data
Tempering: No data
Diagram note: Indicative values for 20 mm plate.

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.