Ferro-Titanit C-Spezial Steel
Steel name: Ferro-Titanit C-Spezial
Diagram No.: 2338
Chemical composition in weight %: Carbide phase: TiC, 33%. Binder phase: 0.65% C, 3.00% Cr, 3.00% Mo, Fe is balance.
Steel group: PM cold work tool steels
Properties: The binder phase consists of a cold work steel containing 3% chromium and 3% molybdenum. The relatively low alloy content brings about a low tempering resistance. The hardness decreases above approximately 200 °C. In comparison with the other grades, C-Spezial has the best machining properties.
Applications: All cold work applications in cutting and forming engineering, e.g. for cutting and blanking tools, bending jaws, extrusion punches, deep-drawing dies, form and hobbing punches, clamping jaws, blanking sleeves, tools for the processing of steel, non-ferrous metals, aluminium, etc., as well as machine elements such as pulleys, rollers and guides exposed to heavy wear.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 980 – 1100 C, vacuum, 1 bar N2. Heating to hardening temperature is advisably performed over several preheating stages (e.g. 400 °C, 600 °C, 800 °C) in order to ensure uniform soaking of the parts that are to be hardened and to avoid any cracking induced by thermal stress. The selected soaking time at hardening temperature must be longer than for steel tools (roughly twice to three times). Because of the rigid titanium carbide skeleton, deleterious grain growth as found in tool steel and high-speed steel cannot occur during the heat treatment. It is hence possible to accept slightly higher hardening temperatures and longer soaking times rather than insufficient hardening.
Tempering: 150 C. In order to avoid cracking induced by hardening stresses, parts that have been hardened must be tempered immediately after quenching or cooling to around 50 °C and held at tempering temperature for at least 2 hours, followed by cooling in air.
Diagram note: No tempering temperature other than the one indicated should be selected, as the strong, negative influence on the resistance to wear and pick-up does not justify the minor benefit of toughness improvement.
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.