Cryodur 2550 Steel
Steel name: Cryodur 2550
Diagram No.: 2353
Mat.No. (Wr.Nr.) designation: 1.2550
AFNOR designation: 55WC20
AISI/SAE designation: ~S1
Chemical composition in weight %: 0.60% C, 0.60% Si, 0.35% Mn, 1.10% Cr, 0.20% V, 2.00% W
Steel group: Tool steels
Properties: Impact-resistant oil-hardenable steel, characterized by very good toughness in combination with high hardenability.
Applications: Blanking dies for cutting sheets up to 12 mm thickness, trimming and splitting dies, cold piercing punches, preforming punches, shear blades, chipping knives, pneumatic chisels, coining tools, cold shear blades, ejectors.
Reference: Not shown in this demo version.
Heat Treatment
Hardening: 870 – 900 C, oil or salt bath, 180 – 220 °C.
Tempering: See the diagram.
Diagram note: No data
Tempering Diagram
Price: 20.00 US $
Buy Online Tempering Diagram
Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants
Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.