Formadur 400/Formadur 400 Superclean Steel

Steel name: Formadur 400/Formadur 400 Superclean
Diagram No.: 2361
Chemical composition in weight %: 0.36% C, 0.90% Mn, 1.90% Cr, 0.50% Mo, 0.50% Ni, + additions
Steel group: Plastic mould steels
Properties: Prehardened plastic mould steel with approx. 400 HB. Excellent troughhardenability. Excellent polishability (ESR). Easy machinability. Good weldability. Best texturing properties.
Applications: Plastic mould steel for universal use principal for large-sized complex injection and press moulds. Moulds for e.g. bumpers, tailgates, fenders, spoilers, instrument panels, TV housings. At a supplied hardness of 365 – 410 HB, maximum wear resistance is guaranteed.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 820 – 850 C, polymer or oil.
Tempering: See the diagram.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.