Formadur 2316/2316 Superclean Steel

Steel name: Formadur 2316/2316 Superclean
Diagram No.: 2367
Mat.No. (Wr.Nr.) designation: 1.2316/1.2316
AISI/SAE designation: 420 mod.
Chemical composition in weight %: 0.36% C, 16.00% Cr, 1.20% Mo
Steel group: Plastic mould steels
Properties: Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this steel grade is supplied in a quenched and tempered condition with a working hardness of approx. 300 HB.
Applications: Moulds for processing plastics with corrosive reactions.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1020 – 1050 C, oil or salt bath, 500 – 550 °C.
Tempering: See the diagram.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.