Formadur 2738 Steel

Steel name: Formadur 2738
Diagram No.: 2368
Mat.No. (Wr.Nr.) designation: 1.2378
AISI/SAE designation: P20+Ni
Chemical composition in weight %: 0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo, 1.00% Ni
Steel group: Plastic mould steels
Properties: Pre-hardened plastic mould steel, hardness in as-delivered condition 280 to 325 HB. Good machinability, suitable for texturing, improved through hardening in comparison to Formadur 2711, good polishability.
Applications: Large plastic moulds with deep engravings and intensive impacts on the core. Formadur 2738 is the logical development of Formadur 2311, a pre-hardened plastic mould steel for use in large moulds, which also have to display high core strength. The additional nickel content of 1 % increases through hardening. Formadur 2738 ia a micro-alloyed, vacuum-degassed steel with the following excellent features: good machinability, outstanding polishability, good texturing properties.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 840 – 870 C, polymer or oil.
Tempering: See the diagram.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.