Formadur PH X Superclean Steel

Steel name: Formadur PH X Superclean
Diagram No.: 2369
Chemical composition in weight %: 0.05% C, 15.00% Cr, 4.50% Ni, 3.50% Cu, +Nb
Steel group: Plastic mould steels
Properties: Formadur PH X Superclean is a corrosion-resistant, precipitation hardened steel with high strength. It shows excellent polishability due to the applied remelting process. Compared to Formadur 2316, hardness in as-delivered condition and corrosion resistance are improved.
Applications: Formadur PH X Superclean is recommended for tools used in the processing of corrosive plastics. Further applications for components in aircraft and chemical industries.
Reference: Not shown in this demo version.

Heat Treatment
Formadur PH X Superclean usually is supplied in precipitation-hardened condition with a hardness of 40 HRC.

Ageing Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.