Rapidur 3343 Steel

Steel name: Rapidur 3343
Diagram No.: 2370
Mat.No. (Wr.Nr.) designation: 1.3343
AISI/SAE designation: M2
AFNOR designation: Z85WDCV06-05-04-02
Chemical composition in weight %: 0.90% C, 0.30% Si, 0.30% Mn, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W
Steel group: High speed steels
Properties: Standard high-speed steel grade. Its well-balanced alloy composition forms the basis of its high toughness and good cutting edge retention, rendering it suitable for a large variety of applications.
Applications: For all metal-cutting tools for roughing or finishing such as twist drills, diverse milling cutters, thread dies, broaches, reamers, countersinks, thread chasers, circular saw segments, shaping tools and woodworking tools. Also highly suitable for cold-forming tools such as cold extrusion rams and dies, as well as cutting and precision cutting tools, plastic moulds with elevated wear resistance and screws.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 1190 – 1230 C, salt bath 550 C, oil, air.
Tempering: At least twice 530-560 C.
Diagram note: No data

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The material data is a central depository of information based on global actual tests and calculated software data that is available to the public for a fee. The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2023 by Steel Data. All Rights Reserved.